Availability: | |
---|---|
PDF Export | |
Mat.No. 1.0570/DIN St52-3/AISI 1024
Osaka
Non alloy quality steels: Steels with average C > 0,25 < 0,55 % or Rm > 500 < 700 N/mm2.
Designation by Standards
Mat. No. | DIN | EN | AISI |
1.0570 | St52-3 | - | 1024 |
Chemical Composition (in weight %)
C | Si | Mn | Cr | Mo | Ni | V | W | Others |
max. 0.20 | max. 0.55 | max. 1.60 | - | - | - | - | - | - |
Application
Materials for rail vehicles. Structural steels and structural steels with improved atmospheric corrosion resistance, hot rolled.
Physical properties (average values) at ambient temperature:
Modulus of elasticity [103 x N/mm2]: 210
Density [g/cm3]: 7.85
Normalizing temperature
890-950oC.
Forging
Hot forming temperature: 1050-850oC.
Forms manufactured
Please see the Dimensional Sales Program.
Disclaimer
The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available. Unless otherwise specified, registered trademarks are property of Metal Ravne company. Copyright 2015 by Metal Ravne. All rights reserved. Contact our Sales Office for more information.
Non alloy quality steels: Steels with average C > 0,25 < 0,55 % or Rm > 500 < 700 N/mm2.
Designation by Standards
Mat. No. | DIN | EN | AISI |
1.0570 | St52-3 | - | 1024 |
Chemical Composition (in weight %)
C | Si | Mn | Cr | Mo | Ni | V | W | Others |
max. 0.20 | max. 0.55 | max. 1.60 | - | - | - | - | - | - |
Application
Materials for rail vehicles. Structural steels and structural steels with improved atmospheric corrosion resistance, hot rolled.
Physical properties (average values) at ambient temperature:
Modulus of elasticity [103 x N/mm2]: 210
Density [g/cm3]: 7.85
Normalizing temperature
890-950oC.
Forging
Hot forming temperature: 1050-850oC.
Forms manufactured
Please see the Dimensional Sales Program.
Disclaimer
The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available. Unless otherwise specified, registered trademarks are property of Metal Ravne company. Copyright 2015 by Metal Ravne. All rights reserved. Contact our Sales Office for more information.