Mat.No. 1.1165/DIN 30Mn5
Non alloy special sructural steels: Structural steels with average C < 0,50%.
Designation by Standards
Mat. No. | DIN | EN | AISI |
1.1165 | 30Mn5 | - | - |
Chemical Composition (in weight %)
C | Si | Mn | Cr | Mo | Ni | V | W | Others |
0.31 | 0.28 | 1.35 | max. 0.30 | - | - | - | - | - |
Applications
Quenched and tempered steel castings or general engineering uses.
Physical properties (average values) at ambient temperature
Modulus of elasticity [103 x N/mm2]: 210
Density [g/cm3]: 7.85
Normalizing
Heat to 870oC, cool slowly.
Hardening
Harden from a temperature of 840oC followed by water or oil quenching.
Tempering
Tempering temperature: Please ask.
Forging
Hot forming temperature: 1050-850oC.
Forms manufactured
Please see the Dimensional Sales Program.
Disclaimer
The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as it become available.
Unless otherwise specified, registered trademarks are property of Metal Ravne company. Copyright 2015 by Metal Ravne. All rights reserved. Contact our Sales Office for more information.
Non alloy special sructural steels: Structural steels with average C < 0,50%.
Designation by Standards
Mat. No. | DIN | EN | AISI |
1.1165 | 30Mn5 | - | - |
Chemical Composition (in weight %)
C | Si | Mn | Cr | Mo | Ni | V | W | Others |
0.31 | 0.28 | 1.35 | max. 0.30 | - | - | - | - | - |
Applications
Quenched and tempered steel castings or general engineering uses.
Physical properties (average values) at ambient temperature
Modulus of elasticity [103 x N/mm2]: 210
Density [g/cm3]: 7.85
Normalizing
Heat to 870oC, cool slowly.
Hardening
Harden from a temperature of 840oC followed by water or oil quenching.
Tempering
Tempering temperature: Please ask.
Forging
Hot forming temperature: 1050-850oC.
Forms manufactured
Please see the Dimensional Sales Program.
Disclaimer
The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as it become available.
Unless otherwise specified, registered trademarks are property of Metal Ravne company. Copyright 2015 by Metal Ravne. All rights reserved. Contact our Sales Office for more information.